jasmin Posted August 23 Report Share Posted August 23 (edited) Is there any saving them? He has his dog running loose (which I hate because I do have farm animals and the dog is aggressive) and it got into our yard and peed on my shelves. I just noticed it today but he was in the kiln room over a week ago. I thought he had missed them but I went to fire today and smelled it. I have searched online but have gotten no answer. I don’t have the funds right now to purchase more 😭 Edited August 24 by jasmin Quote Link to comment Share on other sites More sharing options...
Bill Kielb Posted August 23 Report Share Posted August 23 My take - bisque fire them, burnout all organics Rae Reich 1 Quote Link to comment Share on other sites More sharing options...
jasmin Posted August 24 Author Report Share Posted August 24 Thank you so much for the response. I will bisque them. Bill Kielb 1 Quote Link to comment Share on other sites More sharing options...
Mark C. Posted August 24 Report Share Posted August 24 (edited) Yes bisque them. They will smell on the heat up then be fine. If the dog or cat ever pees on your kiln use natures miracle to remove smell.It works well Edited August 25 by Mark C. Rae Reich 1 Quote Link to comment Share on other sites More sharing options...
Hulk Posted August 24 Report Share Posted August 24 ...check the weather model for predicted wind direction... Kelly in AK, PeterH and Rae Reich 3 Quote Link to comment Share on other sites More sharing options...