Hello! I am having trouble with my new kiln relays. When i turn on my kiln, all the elements heat up, but the relays keep firing super quickly and sound like a machine gun. Any idea what is wrong with them? I have fired successfully with them in the past. 

Edited by Josh125
Link to comment
Share on other sites

I don't typically see relays chatter when they're failing, but it's possible. If they're all chattering then it's more likely a controller issue. If you just replaced them then it could be a wire in the wrong place. The other thing that comes to mind is if the controller somehow got set for solid state relays. What brand and model kiln is it, and what type of controller?

Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.