TracyH Posted July 13 Report Share Posted July 13 Hello everyone, Does anyone know where I can purchase Norwegian Nepheline Syenite? I am in Canada. Cannot find this anywhere. It cannot be substituted with regular syenite. Thank you Quote Link to comment Share on other sites More sharing options...
Callie Beller Diesel Posted July 13 Report Share Posted July 13 I don’t know that any of the Canadian suppliers import it, but if you have a brand name, we can help you substitute it in your recipes. There’s a few of us that are handy with glaze software like that. Quote Link to comment Share on other sites More sharing options...
PeterH Posted July 13 Report Share Posted July 13 Digitalfire gives an analysis for Norwegian Nepheline Syenite aka Norwegian Nepheline Syenite aka Spectrum N500. https://digitalfire.com/material/nepheline+syenite+norwegian Quote Link to comment Share on other sites More sharing options...
Mark C. Posted July 13 Report Share Posted July 13 (edited) The regular A270 Nep Sy is really close to the Norwegian stuff. Not worth the effort in my view Edited July 14 by Mark C. Quote Link to comment Share on other sites More sharing options...
Recommended Posts
Join the conversation
You can post now and register later. If you have an account, sign in now to post with your account.