making colored clay

Recommended Posts

Would someone be so kind as to walk me through the making of colored clay preferably with already manufactured ingredients like mason stains. Some years back I tried adding the powdered stain directly into my clay body but with only minimal success... What has worked for you?

Share this post


Link to post
Share on other sites

When I color my clay, one of the easiest ways I usually do it is just to add the mason stains to my slip in my scrap buckets and blend in with a jiffy mixer. simple. When you reclaim as normal ... you have an easier time wedging.

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.