Marie1234 Posted January 15 Report Share Posted January 15 Hi everyone, I want to glaze some bisque plates with Amaco HF9 clear glaze. I tried brushing it but it was quite thick and didn’t flow easily. It also smudged the underglaze. I have read that dipping is a much better technique to achieve a uniform/clean finish and not ruin the underglaze. Do I need to add water/anything else to the glaze to use it for dipping please? If so, how much? Thanks! Quote Link to comment Share on other sites More sharing options...
Min Posted January 15 Report Share Posted January 15 Is the glaze made for brushing or dipping? Quote Link to comment Share on other sites More sharing options...
Marie1234 Posted January 15 Author Report Share Posted January 15 Hi Min, In the label it says it can be applied both ways. Quote Link to comment Share on other sites More sharing options...
Marilyn T Posted January 16 Report Share Posted January 16 I mix it to a SG of 1.45 for dipping or spraying and it worked well on white clays over slip/underglaze. I haven't tried brushing. On brown clay, not so successful -- lots of bubbles that didn't clear (experiment in process). Min 1 Quote Link to comment Share on other sites More sharing options...
Recommended Posts
Join the conversation
You can post now and register later. If you have an account, sign in now to post with your account.