A friend just contacted me with the sad news of the passing of a dear friend of hers. She has been charged with the responsibility of making an urn for his ashes and would love to use horse hair decoration. I assume she must mean horse hair raku and I have no familiarity with the technique. Do any of you have any suggestions that would be helpful, firing temperature, type of clay, how much horse hair, etc? Thank you for being a deep pond of knowledge, Joan Klotz.

Share this post


Link to post
Share on other sites

A friend just contacted me with the sad news of the passing of a dear friend of hers. She has been charged with the responsibility of making an urn for his ashes and would love to use horse hair decoration. I assume she must mean horse hair raku and I have no familiarity with the technique. Do any of you have any suggestions that would be helpful, firing temperature, type of clay, how much horse hair, etc? Thank you for being a deep pond of knowledge, Joan Klotz.

 

 

www.pyromaniapottery.ca is a wonderful studio gallery on Vancouver Island Canada... one of their potters makes incredible horsehair pots, and I'm sure that she would be more than happy to assist you.

 

 

Flora Walton

 

 

Share this post


Link to post
Share on other sites

Horse hair decorating is done at a much lower temperature (1100-1200 F or so) than raku 1850 F.
The piece is removed and long horse tail hairs are contacted with the hot surface which carbonizes into the surface. One or two hairs at a time quickly before the piece cools.
The surface is usually burnished with terra sig prior the bisque firing (^09)

For a burial urn, I would think you would want a vitrified clay body. The horse hair is porous and soft by the nature of the process.

Marcia

http://ceramicartsdaily.org/potters-council/alternative-firing-surfaces/

Share this post


Link to post
Share on other sites

Use a fine grained clay body, and burnish it before firing. Heat to 1200F, pull it from the kiln, add the horse hair QUICKLY, then cover it with a bucket to slow the cooling. Wash it down after it cools, let it dry for a couple of days, then wax and buff the surface with any car wax.

Share this post


Link to post
Share on other sites

Use a fine grained clay body, and burnish it before firing. Heat to 1200F, pull it from the kiln, add the horse hair QUICKLY, then cover it with a bucket to slow the cooling. Wash it down after it cools, let it dry for a couple of days, then wax and buff the surface with any car wax.

 

 

 

Thanks very much for this concise and helpful reply, Neil, I too was under the impression that raku firing was required

Christine

Share this post


Link to post
Share on other sites

Use a fine grained clay body, and burnish it before firing. Heat to 1200F, pull it from the kiln, add the horse hair QUICKLY, then cover it with a bucket to slow the cooling. Wash it down after it cools, let it dry for a couple of days, then wax and buff the surface with any car wax.

 

 

 

Thanks very much for this concise and helpful reply, Neil, I too was under the impression that raku firing was required

Christine

 

 

It is like raku firing in that you're pulling the piece from the kiln while still hot, but you're not doing the post-firing reduction. One word of warning- if you get too much hair trapped under the cooling bucket, it can cause some reduction and grey out the surface. Before you cover it make sure there's very little unburned hair in there.

Share this post


Link to post
Share on other sites

Use a fine grained clay body, and burnish it before firing. Heat to 1200F, pull it from the kiln, add the horse hair QUICKLY, then cover it with a bucket to slow the cooling. Wash it down after it cools, let it dry for a couple of days, then wax and buff the surface with any car wax.

 

What kind of clay are you using when you do this?

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.