Can someone advise when is the best stage of drying to carve porcelain? I have just started throwing and handbuilding with porcelain and not sure whether it is leather hard or dry.

 

Thanks Annie

Share this post


Link to post
Share on other sites

The most important thing is to limit the amount of dust that you will create.

You have to determine the best texture for your carving.

Try carving at different 'water content textures' and see what feels best to you. Get a spray bottle just incase you may need to add a little water.

Share this post


Link to post
Share on other sites

The answer lies with what you want your carving to look like as each stage will give you a different look. As your porcelain dries your lines will go from soft and flowing to sharp and precise. Also, every type of porcelain will react a bit differently at each stage with some being more forgiving than others.

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.