MMFOWV Posted July 26, 2010 Report Share Posted July 26, 2010 Can anyone give me a cost effective brand name and source for spray guns/ spray booth to use in glaze application? Are the bottom cannister spray guns better/easier to handle when spraying for an extensive length of time? Link to comment Share on other sites More sharing options...
Seasoned Warrior Posted July 26, 2010 Report Share Posted July 26, 2010 Can anyone give me a cost effective brand name and source for spray guns/ spray booth to use in glaze application? Are the bottom cannister spray guns better/easier to handle when spraying for an extensive length of time? my personal favorite is he Paasche 62, check it out at http://www.chicagoairbrushsupply.com/pa62sphe.html I've also seen a lot of ggod thinggs about a detail sprayer with a gravity feed available Habor Freight. I've never used it but a lot seem to like it. I think the orifice would be too small and glog frequently but a lot do like it. The Paasche uses less air and you can use a variety of bottles on the siphone. I like the squeeze type ketchup bottles one finds in a restaurant (or restaurant supply house) which are cheap and are larger than the the one that comes with the sprayer. You also need to replace the small pick-up tube because with the larger bottles it too short. great sprayer, easy clean up and failproof. Regards Charles Link to comment Share on other sites More sharing options...
ArtView Posted July 28, 2010 Report Share Posted July 28, 2010 Great spray gun from Bailey. Advantage is the mechanical parts do not wear out from glaze chemicals...also, does not clog as often. Tip: buy extra containers for quick glaze changeovers. Bailey Spray Gun Based on research, this is my favorite spray booth....depends on your needs: Spray Booth and if you are pretty handy...a homemade idea....(my understanding is that you can get really creative with a squirrel cage - I think that is the name--from an HVAC parts supplies/company) Homemade spray booth Good luck!! Link to comment Share on other sites More sharing options...
Marcia Selsor Posted July 29, 2010 Report Share Posted July 29, 2010 I use an "E-Z" sprayer that I got from Archie Bray Clay business ages ago. I have 4 additional jars for quickly changing glazes while spraying. It is a simple syphon sprayer/ I also use a Paasche air brush for applying underglazes. I have an old power pal compressor from Sears that I have also had for ages. Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.