I just had a full kiln load of bisque Way over fire. It was suppose to fire to 06 but went to at least cone 8.

I connected the wires wrong to the thurmo couple & everything came out burnt.

 

** Question. I know for raku, the clay needs to be open & UN vitrafied.

Will it still be Ok to Raku without cracking?

 

 

Thanks,

Share this post


Link to post
Share on other sites

I'm not sure what burnt means. If you are using a clay formulated for raku, which is usually a low fire clay, and you reached cone 8 your pots should be slumped or puddled all over your kiln. I would think that you will have a lot more difficulty getting enough glaze on the pieces to form glass and getting the smoked black on the unglazed areas than problems with cracking the pots. It is possible to refire cone 10 electric glaze fired pots in a raku kiln to reduce them so I wouldn't think firing to raku temperatures with pots already fired way past the normal firing temperature for raku would cause that big a problem with cracking. I know people who bisque to 04 for raku and then fire the glaze to a slightly lower temperature and they come out even though the clay was vitrified in the bisque. Simplest way to tell is try to fire them and see what happens.

Mike

Share this post


Link to post
Share on other sites

Actually, good raku clay should be a high fire clay, cone 6 upward. It stays open becasue it does not vitrify. If you fired to cone 8, your clay is probabluy a cone 10 clay and, therefore, close to vitrification at cone 8. You may still be able to get some light carbon markings and reduction that could be very interesting and subtle. It would be interesting to try splashes of slip resist and heavily reduce in sawdust to see what happens. I am imagining lovely cloudy greys. If you do dercide to give it a try, let us know and post pictures. Good luck.

Share this post


Link to post
Share on other sites

I have refired a number of pieces that were made with raku clay. The trouble usually comes in the 650 to 900 degree F. range. you might give some thought to salt fuming or pit firing. Please let us know how it turns out.

Share this post


Link to post
Share on other sites

I'm very new to raku.

 

I find raku clay very versitile and can fire high or low temps. I would still experiement with raku clay fired to cone 8, if no carbone trapping I would then glaze and fire again using say cone 10.

Can someone tell me the best bisque temp to fire raku?

Share this post


Link to post
Share on other sites

Hi Linnet,

 

I bisque fire my Raku pieces to cone 06 - basically the same temp as the Raku final fire. Then glaze/tape/naked raku or whatever other decorating technique, and do the final Raku fire at around 1800 F for most pieces before reduction. Not sure if this temp applies to all Raku clays, but at least it seems to work well for the Raku clay I'm using.

 

Best wishes!

Carl

Share this post


Link to post
Share on other sites

I just had a full kiln load of bisque Way over fire. It was suppose to fire to 06 but went to at least cone 8.

I connected the wires wrong to the thurmo couple & everything came out burnt.

 

** Question. I know for raku, the clay needs to be open & UN vitrafied.

Will it still be Ok to Raku without cracking?

 

 

Thanks,

 

If you really did hit ^8 then the clay will be too vitrified to withstand the thermal shock of a raku firing and it will crack.

Sorry.

 

 

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.