azglp Posted October 4, 2022 Report Share Posted October 4, 2022 (edited) Hi We are having an issue with applying the same color for the text Cafe Beirut and the arabic text. The text color looks the same before firing, while after firing the Cafe Beirut text appears softer than the arabic text. Edited October 4, 2022 by azglp Quote Link to comment Share on other sites More sharing options...
Babs Posted October 4, 2022 Report Share Posted October 4, 2022 !!Is it illusionary because of amount of white surrounding the arabic text compared to the compact Cafe Beirut design? Piedmont Pottery, Rae Reich and PeterH 3 Quote Link to comment Share on other sites More sharing options...
azglp Posted October 4, 2022 Author Report Share Posted October 4, 2022 Yes it probably is. I will try applying a darker shade for the english font Rae Reich 1 Quote Link to comment Share on other sites More sharing options...
PeterH Posted October 4, 2022 Report Share Posted October 4, 2022 17 minutes ago, Babs said: !!Is it illusionary because of amount of white surrounding the arabic text compared to the compact Cafe Beirut design? A very good idea. Which I tried to confirm by picking up the colours in graphics program, but they do seem different. Quote Link to comment Share on other sites More sharing options...
azglp Posted October 4, 2022 Author Report Share Posted October 4, 2022 We are comparing the color on Cafe Beirut font and the Arabic Text. The wave color pattern is a different color 2 minutes ago, PeterH said: A very good idea. Which I tried to confirm by picking up the colours in graphics program, but they do seem different. Quote Link to comment Share on other sites More sharing options...
Babs Posted October 4, 2022 Report Share Posted October 4, 2022 Have you a test tile you could apply both graphics side by side? I actually "see" the Cafe Beirut as darker already.... Hulk 1 Quote Link to comment Share on other sites More sharing options...
PeterH Posted October 4, 2022 Report Share Posted October 4, 2022 3 minutes ago, azglp said: We are comparing the color on Cafe Beirut font and the Arabic Text. The wave color pattern is a different color Oops, in that case Babs is right. Hulk and Piedmont Pottery 2 Quote Link to comment Share on other sites More sharing options...
azglp Posted October 4, 2022 Author Report Share Posted October 4, 2022 Thank You @PeterH @Babs Quote Link to comment Share on other sites More sharing options...