Kakes Posted April 25, 2022 Report Share Posted April 25, 2022 Hi everyone, I just fired my kiln (skutt 1222) & after unloading it, realized I forgot to fire a piece. Duh. So now, I have to fire it by itself. It’s a sculpture about 10” x 6”. Should I adjust my firing schedule in some way since the kiln will be practically empty? I normally fire to cone 5 with a 20 minute hold. Also this is a refire where I’ve added another layer of underglaze (fires to cone 5-10) so I only need the underglaze to “cure”, or whatever the right word is. Thanks for any advice! Quote Link to comment Share on other sites More sharing options...
Babs Posted April 26, 2022 Report Share Posted April 26, 2022 Really need it so fast? Waste of power elements etc. Can do it but there could be a fast cool to contend with because of less load mass. Not familiar with your kiln but can take it up at same rate. Pyewackette 1 Quote Link to comment Share on other sites More sharing options...
Callie Beller Diesel Posted April 26, 2022 Report Share Posted April 26, 2022 If you’re only adding underglaze and you intend to go over it with glaze later, you could just put it in your next bisque, unless you need it right away for something. Pyewackette 1 Quote Link to comment Share on other sites More sharing options...
Recommended Posts
Join the conversation
You can post now and register later. If you have an account, sign in now to post with your account.