Dear John,

 

I am sorry to write this to you on this open forum but wanted to let you know that your tip on getting my shelf sandblasted worked like a dream. A guy at a local autobody shop did a quick spray of my shelf and it is as good as new.

 

Cost was $20.00. Sure beats me out there with the chisel and hammer.

 

I will, however, invest in the grinder.

 

Thank you. Another great tip and I can now likely fire without fear tomorrow night.

 

Nelly

Share this post


Link to post
Share on other sites
Guest JBaymore

Thanks :) .

 

If you shop around... you should be able to find that kind of thing cheaper too, I'd bet.

 

best,

 

.................john

Share this post


Link to post
Share on other sites

Thanks :) .

 

If you shop around... you should be able to find that kind of thing cheaper too, I'd bet.

 

best,

 

.................john

 

 

Thank you again. The kiln wash brushed over the new shelf with total ease. I am good to go!!! I am in between teaching semesters so paying $20.00 bucks sure made me happy. It beats spending a lot more on new shelf. Gawd I love this forum....!!! You are the best Mr. Baymore!

 

Nelly

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.