I'm wanting to reduce my energy consumption by going to cone 6 fire.   Previously I've fired to cone 8-9, and i have quite a bit of stoneware, porcelain and high fire slip that I want to use up.

Can anyone tell me what negative results will happen to high fired clays and slips fired to 1200C?

Many thanks

Southern Ice Sue

Link to comment
Share on other sites

On 10/13/2021 at 6:52 PM, Southern Ice Sue said:

what negative results

What Bill said--I have had no luck/success at all trying to find "an easier, softer way" ---with few exceptions (not including intentional experimentation or deliberate applications for artistic purposes)---  my attempts to use materials outside of their tested, identified boundaries have usually gone down a dead end.

Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

 Share

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.