Hi all,

Anyone mix mason stain into their slips regularly?
I mix them thoroughly (good 15 minutes in a mixer) but continue to have streaking where some part of the finished has the stain color, but some do not.
Resulting in an unsightly streaking wherever it's sponged or sanded. Will post pic in a few. Does this ring a bell for anyone?

Link to comment
Share on other sites

@moh, try sending a pm to @Jeff Longtin and asking him. I've only done a bit of coloured slip casting. Haven't had the problem with streaking, I mix the stain with a little water then add it to the slip, mix then put it through a 60 mesh sieve and adjust if necessary. Unglazed and sanded outside black tumbler below, I've used 5 different stains like this with no problems.

DSC_0206.jpeg.29f987e695f0ef218de778e292682670.jpeg

Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

 Share

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.