I am have a pretty wacky issue with my 5 gallon of dippable True Celedon Potters Choice Glaze.

I mixed the original batch and waited the 24 hours.  Mixed again and use.  Came out awesome on a 2x4 platter I made.   

Next time, about 2-4 days later, I went to mix the glaze (using my drill mixer) all the glaze clumped into a hard packed mess at the bottom.  I cannot stir as it seams to have solidified.  I can get the mixer to break it up and was able to do it once.  Next time, same thing.  

Anybody else have this issue.  

KenB

Link to comment
Share on other sites

Maybe someone with direct experience will answer but since this is a commercial glaze we have no idea of how much clay it might contain and if it is naturally deflocculated due to sodium. I suggest a good read for this  https://suemcleodceramics.com/how-to-fix-a-hard-panned-glaze-with-epsom-salts/

You likely will end up using Epsom salt a little at a time to re suspend the glaze. Since bentonite can generally be added up to 2%, you might settle on 1% addition because you will never know the actual clay content, then flocculate with minimal Epsom salt as a start.

Hopefully someone has direct experience with this commercial glaze for a tried and true solution. Actually a call into Amaco probably gets you the most tried and true solution for this glaze. I am sure they have seen it before.

Edited by Bill Kielb
Link to comment
Share on other sites

Adding Epsom salt (or vinegar) to adjust thixotropy has been key turning glazing from chore to joy; here's Tony Hansen's video on the subject:

How to Gel a Ceramic Glaze - YouTube

Reducing "hard panning" is a side benefit for me; perhaps a nice "Gel" behaviour would be a side benefit for you Ken B? If you do increase the thixotropy, reducing specific gravity somewhat may be in order.

Link to comment
Share on other sites

I would reach out to Amaco and ask them if they have any recommendations before making adjustments to your bucket. If the glaze already has some bentonite in it, adding more is going to not help, as a for instance.

If you haven’t got the patience to wait for an email back, mix up your bucket again, and take some samples out to adjust as per the suggestions above (love Sue McLeod!). You don’t want to accidentally mess up your entire bucket.

 

Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

 Share

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.