@Piedmont Pottery  @Callie Beller Diesel @Min sometime way back I was working with some calcium silicate materials as part of a glaze research project.  The problem was how to prevent the calcium silicates forming "concrete" from the glaze slurry sitting still for several days.  The answer came from a Professor researching concrete; very small amounts of sugar are often added to the concrete mix when the pour is more than an hour from the mix station to the pour sight;  using that data, and