Neon glaze colors (bright colors) generally exist  more so in lowfire glazes. I am not sure what is meant by neon other than bright color. Maybe Take a look here and see if this satisfies your color requirements https://www.maycocolors.com/color/low-fire-glazes/ There are some bright colors in underglazes as well. Again lowfire products  often can be brighter than mid or high fire products. https://www.amaco.com/t/glazes-and-underglazes/underglaze/velvet-underglaze/velvet-underglazes

Edited by Bill Kielb
Link to comment
Share on other sites

2 minutes ago, ashhorth said:

Yes fluorescent

Oh dear, I know people have made  [slight] progress with the other two application areas, but I am unaware of anything for day-glow (daylight fluorescent).

PS I will be delighted to be corrected, but I suspect that [all?] day-glow dyes are organic (and presumably incapable of surviving firing). While rare-earth pigments apparently require UV-lighting to glow.

DayGlo® Fluorescent Pigments https://tinyurl.com/3mr9ztdc

In the Studio: Rare-Earth Oxide Glazes https://tinyurl.com/k822vt4v

Link to comment
Share on other sites

I agree with Peter. I think the closest thing we get in ceramics is the rare earth oxides. I’ve seen that pink/purple glaze from the link above  in person. It changes colour in different lights and is *really* cool, but it wasn’t technically fluorescing, I don’t think. I also have a yellow glaze that I get from a praseodymium-based mason stain. While it’s a bright sunny yellow, it doesn’t fluoresce under black light. 

Link to comment
Share on other sites

An order!

What price are you prepared to pu o  your pots which will require such research?

If the understains mentioned above do not suit, I'd walk away from order.

Folk not into ceramics do not understad whst goes into such requests.. 

Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

 Share

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.