Mixing different porcelain


Recommended Posts

If its the glassy(they glassify) porcelains do not mix with non glassy ones. Ones like frost from New zealand are never to be mixed as they are extrremely glassy

Run of the mill ones usually are not an issue to mix

I know nothing of ming in the UK