Kiln venting systems are not only a way to move fumes out of the room, they are also moving the air

inside the kiln to keep firings temps more even throughout the kiln.

 

Fans also helps with even cooling ...

I fire down to control the cooling speed with the fan going all the time. Most cracking and warping

problems happen on the way down.

 

I believe these systems optimize your kilns performance.

Share this post


Link to post
Share on other sites

I have to second Chris on that. An envirovent is well worth the money. It evens out the firing, brightens the colors, and takes nasty gasses out of your workspace. Even bisque offgasses toxins in firing, and some glaze ingredients (like manganese) can be more dangerous to breathe than to handle.

 

I believe there are lots of gadgets potters don't need in the studio. Safety equipments and kiln vents are the exceptions.

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.