I have access to some real Albany Slip and was thinking I'd play around with it in a few glazes. It looks like the best case result would look like a Tenmoku glaze, is that correct? Just trying to figure out if it's worth the hassle, when my Tenmoku is already tried-and-true. Thoughts? Thank you!

Snzanne

Link to comment
Share on other sites

Albany alone at cone 10 is pretty sweet -Making it a Tenmoku is a bit of a waste (adding iron)

If its cone 6 Roberta pegged it above -just do a few small sample tests to dial it in.

Link to comment
Share on other sites

  • 3 weeks later...

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

 Share

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.