Valeria Posted May 18, 2021 Report Share Posted May 18, 2021 Hi! I would like to explore new techniques of decorating with clay, instead of glaze, handbuilding and for surfaces/slabs. I attach a photo to give you an idea. do you have experience with these techniques? How to achieve the circle in the slab for exemple? many thanks, Valeria Link to comment Share on other sites More sharing options...
Babs Posted May 18, 2021 Report Share Posted May 18, 2021 1 hour ago, Valeria said: Hi! I would like to explore new techniques of decorating with clay, instead of glaze, handbuilding and for surfaces/slabs. I attach a photo to give you an idea. do you have experience with these techniques? How to achieve the circle in the slab for exemple? many thanks, Valeria Search Nerikomi and neriage Link to comment Share on other sites More sharing options...
Valeria Posted May 18, 2021 Author Report Share Posted May 18, 2021 Thank you! I know Nerikomi but not neriage. I am having a look and it seems just what I am after. Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.