Natural Minerals C-98 Talc is no longer in production. They have closed their doors to external sales. This is the grey Texas talc that many have been using for decades , it fires white. Laguna Clay Company has a rationed amount for customers still. I'm not user myself as I use another talc that costs more. If you need this talc in a glaze you better stock up NOW.