I would like to make a "reclaim bat", i.e. a tray on which I can lay wet clay/slip so that the water absorbs out of it for eventual re-use.  Should I use pottery plaster or plaster of paris?  And why?

Link to comment
Share on other sites

2 hours ago, Rick Wise said:

I would like to make a "reclaim bat", i.e. a tray on which I can lay wet clay/slip so that the water absorbs out of it for eventual re-use.  Should I use pottery plaster or plaster of paris?  And why?


Once upon a time, I had the same situation, how to reclaim clay and then dry the clay back to throwing moisture.  I used a set of large red clay flower pot plates, or a large flower pot sitting on a flower pot plate.  These remove water just like plaster, are not as heavy, and are cheap.  And no, the red did not contaminate the white (aka porcelain) reclaim.  

LT

Link to comment
Share on other sites

I made a slab out of POP and one out of  #1 pottery plaster.   Someone gave me the POP,  I have always used #1,  it was one of those I need to use up this POP moments.  I decided to make a slab also the same size out of #1 plaster.   Clay on the POP took forever to absorb into the plaster and after several uses it started to crumble.   I also took longer to dry out.   If someone offered me a bag of POP I would kindly refuse it.   Denice

 

Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

 Share

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.