I am looking at upgrading my skutt kilns to the newer touchscreen interface. Pretty straight forward process. But can you use one of these interfaces on on a competitors kiln. I have a couple old olympics of similar size, ect to a 1027. They are about to become, individually zoned, relayed, ect. Perfect time for an upgrade. I know Bartlet has the Genesis programer, but I like continuity if I can get it.

Link to post
Share on other sites

The Skutt non-touchscreen controller is bigger than the standard Bartlett controller. The touchscreen upgrade has a mounting plate that fits the larger Skutt hole. You could probably put in on your other kilns, but you'd have to drill new holes. Take a look at the installation instructions for the Skutt and make sure there isn't something that would be a problem. The Genesis controller is less expensive than the Skutt upgrade. 

Link to post
Share on other sites

I had to build my own box for the olympic controller, so I could get zone control. I'm trying to just mount it to the wall, or a pedestal, so the mount isn't much of a concern. I used a skutt control box rewire kit to build it, because I always have spares. My only wonder, for now lol, is the difference in resistance between the two kilns elements. I couldn't find any info on the olympic 2327 element resistance. Skutt, no problem

Link to post
Share on other sites
1 hour ago, Johnmicheal said:

My only wonder, for now lol, is the difference in resistance between the two kilns elements. I couldn't find any info on the olympic 2327 element resistance. Skutt, no problem

Do you mean in terms of the controller? The controller doesn't care about the elements, it just has to switch the relays.

Link to post
Share on other sites
  • 2 weeks later...

The Genesis is cheaper, but my wife's sanity has value also. It'll be easier for her to fire if there is continuity between the various kiln bodies we have. I don't really care about the app stuff, I've had wifi cameras on my kilns for a couple years. But I do like the very visual way of creating, and tracking our programs. 

 

Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.