Hello everyone. So I glazed a piece and it ran....so now the piece isn't sitting stably. 

I created a wooden base for it to be able to sit comfortably in, but I need an adhesive to attach the glazed piece to this wooden base. Does anyone know of a glue that I can use to achieve this? 

Thanks in advance!

Link to post
Share on other sites

precious, is the run on the bottom?   can you use a grinder to make it flat so it can sit correctly?    in some cases, that is the simplest way to correct a glaze run.

a wooden stand is fine if it enhances the design.  however, if you ever anticipate washing the piece in water, gluing it together will make that extremely difficult.

Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.