Krishugg Posted March 29, 2021 Report Share Posted March 29, 2021 I purchased an item at a ceramic store. A customer has commissioned the piece. She wants it glazed. Problem is, it has a huge unforseen hot spot. The glaze won't stick. I'm afraid it will not fire evenly. Directly in the eyes center gaze! Can I scruff it up? Is there anything to be done? I sure don't want to make it worse. Link to comment Share on other sites More sharing options...
Babs Posted March 30, 2021 Report Share Posted March 30, 2021 Post a pic to help clarify. Link to comment Share on other sites More sharing options...
Min Posted March 30, 2021 Report Share Posted March 30, 2021 Just to clarify you bought a bisque piece that has a hard/hot spot and are trying to glaze it for a customer? If that's right I'ld take it back and get a replacement piece. Link to comment Share on other sites More sharing options...