Dabston Posted March 22, 2021 Report Share Posted March 22, 2021 Trying to make a cone 6 porcelain slip like the old seeley slip. They are out of business now and I want to know where to find the formula they used. Recipe, site to see info Greatly apprecialed Quote Link to comment Share on other sites More sharing options...
neilestrick Posted March 23, 2021 Report Share Posted March 23, 2021 Their formula was likely proprietary information, so I'm not sure where you would find it. Are you just looking for a good cone 6 porcelain recipe, or is there some specific feature of their porcelain you're after? There's also THIS. Quote Link to comment Share on other sites More sharing options...
Dabston Posted March 23, 2021 Author Report Share Posted March 23, 2021 Do you have a recipe for cone 6 porcelain slip. One Using tile 6 one using EPK. Also need a recipe for stoneware. Thank you Quote Link to comment Share on other sites More sharing options...
Jeff Longtin Posted March 27, 2021 Report Share Posted March 27, 2021 I was introduced to Seeley and Bell Porcelain slip back in the 90's. (When I made a few molds for doll artists.) I found both to be very white and very vitreous. I also noticed that both developed green mold fairly quickly. Recently I've returned to mixing my own and found that recipes that use English Grolleg Kaolin have the same qualities. (Whereas recipes with EPK or #6 Tile do not.) A recipe from claybucket.com is proving to work nicely. 10,000 gms water 80 gms Darvan 100 gms Bentonite 11000 English Grolleg Kaolin 4600 Nep Sye 4400 Flint S. Dean 1 Quote Link to comment Share on other sites More sharing options...
Robert Pirrung Posted August 16, 2022 Report Share Posted August 16, 2022 I have a variety of Seeley Porcelain slip, when Rolf was in business, up in Oneida, NY, anybody interested please email soon, otherwise it will be gone. Quote Link to comment Share on other sites More sharing options...
Recommended Posts
Join the conversation
You can post now and register later. If you have an account, sign in now to post with your account.