I have come to understand (from your prior good advice) the importance of knowing the specific gravity of my glazes.  Here is my related question:

Assuming no deliberate additions or subtractions of water or material, is there any reason to expect  a known SG to change other than from:

(1) the natural evaporation of water, or

(2) use of the glaze by dipping in pieces that may take up disproportionate amounts of water or materials?

Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.