The Chinese used to use a high calcium product that make painting in the tortoise shell and partridge feather style possible. I would suggest exploring that.

- h a n s e n

Share this post


Link to post
Share on other sites

I need to create a set of dishes using temoku with another glaze. Any suggestions?

 

 

I like accents with John Reeves Chrome Green.

 

REEVES GREEN cone 10 reduction

CUSTER 75.0

WHITING 15.0

FLINT 5.0

KAOLIN 5.0

CHROME OXIDE 4.0

 

Or, if you'd like something tradtional, put Nuka at the top.

 

*Phil Roger's Synthetic Nuka

 

Potspar 35.6

Whiting 21.8

Talc 2

Bone Ash 2

Ball Clay 5.9

Flint 29.7

ferro3134 3 (I have subbed wood ash) *

 

See photo here: Nuka over Tenmoku

http://images21.fotki.com/v760/photos/1/199764/814063/AUT_0020-vi.jpg

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.