Welcome to the forum @Beliz Çıta

Please update your details and let us know where in the world you are located.  That will help with recommendations of brands etc.

Also, please note that underglaze is underglaze.  Not underglaze paint.  Paint does not go into a kiln.  Or if it does, it rarely ever survives.

Link to comment
Share on other sites

Commercial underglazes can be applied to leather hard, bone dry, or bisque. I prefer to apply them before bisque because then the binders and hardeners burn out in the bisque and they take glaze better. I use Speedball brand underglazes, which are usually the least expensive. All brands work well, though, it just depends on the colors you want and how much you want to pay. Most colors hold up well at cone 6, but you may want to test any colors with the glaze you plan to use to see how they hold up.

Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

 Share

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.