Although I am storing the clay in a large, sealed, plastic container that has a wet plaster bottom (a very moist environment) it remains too hard even after months of storage!  II must be missing something.

Related :   While stored in the plastic container,  is it better to open the bag or keep it closed with the rubber band ?   (Sometimes I have been leaving it open on the theory that the environment in the plastic container is MORE moist than the clay.)

Link to comment
Share on other sites

It’s definitely better to leave the bag closed. The amount of water that was added to the batch can only leave the clay, not return to it when exposed to open air. It’s a different story if you’re using something like the water bucket method to rehydrate the clay, but I don’t think that’s what you’re talking about.

Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

 Share

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.