Hi, I’m using an off the shelf transparent glossy glaze, which has worked really well in the past, it is now creating little air blisters all over everything in the kiln.  I’ve tried higher and lower temps, I’ve tried bisque firing at a higher temp, I’ve tried mixing glaze to dip (with water) and glaze mixed with the brush on medium, I’ve tried one coat, two coats. It is worse on horizontal. Could it be a bad batch of glaze? It’s driving me insane, advise would be greatly appreciated.
 

Edited by Zoewoods
Link to post
Share on other sites
4 hours ago, Zoewoods said:

Hi, I’m using an off the shelf transparent glossy glaze, which has worked really well in the past, it is now creating little air blisters all over everything in the kiln.  I’ve tried higher and lower temps, I’ve tried bisque firing at a higher temp, I’ve tried mixing glaze to dip (with water) and glaze mixed with the brush on medium, I’ve tried one coat, two coats. It is worse on horizontal. Could it be a bad batch of glaze? It’s driving me insane, advise would be greatly appreciated.
Good question, I've had similar problems recently. I suggest reading this page and particularly going down to the section "Limit Formulas" and clicking on the highlighted links for good info. https://digitalfire.com/4sight/education/limit_formulas_and_target_formulas_206.html
Good luck!

 

Link to post
Share on other sites

Hi Zoe!

Could you post pictures - glazed pieces before and after firing? What clay(s) are you using, at what temps? Did the problem(s) onset match up with opening a new/different package of glaze? If so, do you have any of prior/good glaze left to compare with? What brand of glaze (if you're comfortable sharing that...)? Could there be any other factors, e.g., are you working with same clay as before problem? Firing same? Your process same? Is the problem isolated to the one glaze, iow, are you having same/good results with your other glazes?

Edited by Hulk
redundantly saying the same thing over again
Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.