Years ago, I had some pieces that blew out in the bottom. I ground out the base area and created  cup forms for the bases. These did fit together well, and the join area tapered as it was did not look like anything more than an undercut line on the foot ring. It worked, but with all the effort it took, I decided that future problems like that were best solved by throwing a new one. However, the effort taught me a few things about precision, wet/dry shrinkage and joining.

 

best,

Pres

Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.