  Likely a "ball clay" per Pieter Mostert entry in Glazy; see also "G&W B13 Clay" entry in Digitalfire

  G&W B13 Clay (digitalfire.com)

Frit 91076

  Per Bill's response, Digitalfire entry (and Glazy as well):

  Degussa Frit 90167 (digitalfire.com)

  Degussa Frit 90167 | Glazy

I'm not finding Degussa products available stateside - there's some encapsulated stain credited to Degussa, but manufactured by Ferro - however, looks like Keramik-Kraft (Germany) has 90167, and some other suppliers  (Hungary, etc.). 

Any road, back to Jennifer's question, which Feldspar? Are the colorants not listed? What target cone and atmosphere?

Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

 Share

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.