Jump to content

Engobe on bone dry ware


Nicky S
 Share

Recommended Posts

Hi ...... Have some porcelaine cups that have reached the bone dry stage .Am wondering if I can still use engobes or slip on them before bisque firing ? Also can engobes or slip be  used on bisque ware ? and then does one glaze as usual ?

Thankyou Nicky 

Link to comment
Share on other sites

There is often some difference in peoples definition of a slip versus an engobe. Part of my definition between the two is a slip contains more raw clay than an engobe and therefore a slip will shrink more than an engobe. Since your cups are now at the bone dry stage I definitely wouldn't use a slip, it will shrink more than the cups during firing and probably crack or shell off. An engobe would be a possiblity, but they have to be made to fit the body they are going on. Easiest option would be to use an underglaze. They can go on dry greenware or bisque. You can either bisque fire the underglaze on when applied to greenware or bisque or glaze over an unfired underglaze on bisque. The latter method can have glaze absorption issues as underglazes contain binders that can impede glaze application.

Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

 Share

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.