Ninni Posted August 6, 2020 Report Share Posted August 6, 2020 Hi, I wonder if anyone has experience of burning gold a second time? I need to improve in a place where it did not go well. (I am using Duncan Premium) Ninni Link to comment Share on other sites More sharing options...
Bill Kielb Posted August 6, 2020 Report Share Posted August 6, 2020 Yes, have done it successsfully Link to comment Share on other sites More sharing options...
Ninni Posted August 6, 2020 Author Report Share Posted August 6, 2020 Wow! That is beautiful! Thank you! Link to comment Share on other sites More sharing options...