Im pretty new to layering glazes and was looking to create something like the attached image. Before I dive into looking for suitable recipes, I wanted to know how this effect might be achieved. Is it with a runny base glaze and another glaze on the top half? Is it a base glaze + two blue glazes? Just need a direction to explore more. I fire in an electric kiln to cone 6. Thanks

Screen Shot 2020-06-05 at 10.48.22 AM.png

Link to comment
Share on other sites

Looks like a white glaze that contains titanium and zinc over the entire cup, and another glaze brushed around the top.  The color sort of looks like a nickel blue/grey.

Just a shot in the dark since we know nothing except what the photo looks like