Tia Sculpt 0 Posted May 14, 2020 Report Share Posted May 14, 2020 Hello! I was wondering if anyone could make a suggestion since last night I did a bisque fire at 04 cone. When I opened the kiln today the cone was completely straight, however it seemed the kiln did a full fire as I set the timer to 7 hours total and have never gone over that time span. I've used this method many times and have always gotten normal 90 degree bent cones so I was so taken back when the cone appeared as if no firing was done ? Could I of just gotten a defective cone ? I've used about 10 from the same pack with no issues. It's the strangest thing... I've never used witness cones but now I feel I may need too. Thanks for any advice! Quote Link to post Share on other sites
neilestrick 4,586 Posted May 14, 2020 Report Share Posted May 14, 2020 If the timer shut it off, but the cone didn't bend, then the firing didn't get to temp. Either your elements are showing wear and the firing needs longer to complete, or something broke toward the end of the firing, like a switch died or a wiring connection fried out. After you unload the kiln, turn it on high for a bit and see ir all the elements glow. If they do, then it's probably that your elements are starting to wear and the firing need to go longer to reach temp. Ideally you'll want to get a multi-meter and check the resistance of the elements to see what condition they're in. Quote Link to post Share on other sites
Mark C. 4,860 Posted May 14, 2020 Report Share Posted May 14, 2020 (Could I of just gotten a defective cone) extremely small chance-they only go bad if they got wet Quote Link to post Share on other sites
Tia Sculpt 0 Posted May 14, 2020 Author Report Share Posted May 14, 2020 Thanks for you help above! Should I refire the current load after testing my elements? Quote Link to post Share on other sites
Dick White 398 Posted May 14, 2020 Report Share Posted May 14, 2020 I have seen a few rare similar situations where upon close inspection of the sitter, there was something impeding its movement. Check that the sensor bar moves freely, and that the bar itself is not worn or damaged. (I have also seen inadvertent mixups of the cones. An 04 cone is brown both before and after firing, while a mid- or high-fire cone is a pastel color before firing and white afterwards. You probably didn't, but that's what I said the time I did it...) After checking everything, including elements, etc. as noted above by Neil, refire the load - and put some witness cones in so you know exactly what happened on the shelf; just because a sitter drops doesn't always equate to that cone in the middle of the shelf, and if the sitter doesn't drop because of a malfunction, it nonetheless may have reached the intended cone because of the timer. As for refiring the ware, it doesn't change the ceramic in any way if it reaches bisque temperature again, but in the off chance it was underfired before, this will bring it up to where you want it for consistent glazing. Magnolia Mud Research and dhPotter 2 Quote Link to post Share on other sites
oldlady 2,799 Posted May 14, 2020 Report Share Posted May 14, 2020 and, tia, do not reuse the cone you used for this firing, toss it out. Quote Link to post Share on other sites
liambesaw 2,748 Posted May 14, 2020 Report Share Posted May 14, 2020 Don't forget your witness cones! Very important with a kiln sitter, I've had my sitter cone break a little bit and turn off my kiln very early and the only reason I knew something was wrong was that my 05 and 04 witness cones were still fully erect. Quote Link to post Share on other sites
Babs 1,203 Posted May 14, 2020 Report Share Posted May 14, 2020 Same density of load? More kiln furniture? 7 hours pretty short bbisque time to 04. Did you miss a turn up of kiln....Or did it later than usual? Just asking as 7 hrs is pretty short imo. liambesaw 1 Quote Link to post Share on other sites
Smokey2 74 Posted May 15, 2020 Report Share Posted May 15, 2020 What size is your kiln? How soon did you turn the kiln to high? 7 hours for a kiln smaller than 3cuft only half full may be ok. A kiln bigger kiln heavily loaded may be to short On 5/14/2020 at 11:51 AM, Tia Sculpt said: I've never used witness cones but now I feel I may need too. Yes, by all means do. Years back when I was still using a sitter kiln I've seen times when the ^04 sitter cone was straight and the ^04 witness cone was almost touching the shelf. On 5/14/2020 at 12:38 PM, Tia Sculpt said: Should I refire the current load It can't hurt, but lets say if the pots fired to the equivalent to ^06 you should be ok to just go ahead and glaze them. Just remember that the pots will soak up fluid faster so if you are dipping your pots into glaze you may need to dip them for a shorter time. I don't brush so I can't speak to that. Quote Link to post Share on other sites