Newer potter, on my 5th or 6th glaze firing, and my first screw up!

I'm running a glaze fire to cone 6, with my skutt 1027 electric with a bottom vent. I totally forgot to plug the peep holes until I went in after about 5 hours (so about 55% of the way through a normal 'medium' speed run). It was at 1500 degrees. I never leave plugs out because of the vent. I plugged it, but now I'm totally curious if I've messed up the entire batch! All I can see in searches is referencing top holes, and notes that it's not required when you have a vent... but will it cause damage if it gets up to 1500 without plugging and with a vent? I'm prepared for it to take a bit longer to reach temp, but since I won't be opening the kiln until tomorrow night, and help managing my expectations or alleviating my fears would be great!

Thanks!

(Also, since I never leave plugs out, I've never seen the red glow through the holes - don't worry, I didn't look directly at it, but I was like, cooooooool.

Link to comment
Share on other sites

17 hours ago, liambesaw said:

I dunno, I routinely leave my peeps out  because my clay is gassy.  I bet it'll be fine since you caught it before anything started melting. Things might be smoother and nicer than normal, you never know until you open it tomorrow ;)

Question - in my new-to-me manual kiln it states to shut all peepholes when it is on high. I'll be running a glaze run in a couple of days (just waiting for my witness cones) and don't know what to do. It seems to me most people leave one peephole open for the gases to escape. I don't have a vent on my kiln. It's a practically brand new ~6cf Sandstone Skutt kiln with a sitter. I guess I should follow the instructions...but I dunno?

Link to comment
Share on other sites

8 minutes ago, liambesaw said:

Once you have them all on high, you want them closed so the temperature climbs steadily.  Until then you can pull the peeps to get things gas off.

Thanks...when should I open them? After it has turned off? Thanks!

Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

 Share

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.