Hey friends. I’ve been throwing for a while at a community center but just got my own kiln. I threw some pieces on low fire body (cone 06-08) and then stupidly glazed them in a mid fire glaze (cone 5-7). Is there any way to salvage this or fire low fire clay with mid fire glaze without risking messing up my kiln? Any creative solutions/ help are so appreciated! Thank you!!

Link to comment
Share on other sites

Hi Ashley and welcome to the forum.  :)

Wash the glaze off the pots, scrub them well then let them thoroughly dry and start again with your lowfire glazes. Maybe look at this as a blessing in disguise, better to realize the mistake now rather than if you had fired them to midrange and probably would have had to deal with melted clay on your shelves.

Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

 Share

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.