Shino libbys base with a flat shaners red on top.

 

 

 

 

I wash of my bowls I take my time and prep them.  Wait for one to dry then dip it in the other. 

 

 

 

 

Any ideas on how to prevent more crawling or stop it? besides Kiln errors

 

 

 

 

4683329355_d1af31979e_b.jpg

Share this post


Link to post
Share on other sites

Shino libbys base with a flat shaners red on top.

 

I wash of my bowls I take my time and prep them. Wait for one to dry then dip it in the other.

 

Any ideas on how to prevent more crawling or stop it? besides Kiln errors

 

 

 

Shinos crawl because of high clay content and shrinkage.

Adding darvan may reduce the problem.

Share this post


Link to post
Share on other sites

Shino libbys base with a flat shaners red on top.

 

I wash of my bowls I take my time and prep them. Wait for one to dry then dip it in the other.

 

Any ideas on how to prevent more crawling or stop it? besides Kiln errors

 

 

 

Shinos crawl because of high clay content and shrinkage.

Adding darvan may reduce the problem.

 

 

Thank you Sir thank you thank you thank you 

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.