I've never used any stains before. I'm getting ready to start experimenting.

I've been pouring a tumbler cup mold with just plain white porcelain slip, into a plaster mold I made. If I add mason stain to the slip would it stain the plaster mold? If it does, would it effect or contaminate the next pouring w/o stain? I hope that makes sense. I just want to try and color my slip, but don't want it to ruin my plaster mold.

 

Thanks,

Gwen

 

 

Share this post


Link to post
Share on other sites

I've never used any stains before. I'm getting ready to start experimenting.

I've been pouring a tumbler cup mold with just plain white porcelain slip, into a plaster mold I made. If I add mason stain to the slip would it stain the plaster mold? If it does, would it effect or contaminate the next pouring w/o stain? I hope that makes sense. I just want to try and color my slip, but don't want it to ruin my plaster mold.

 

Thanks,

Gwen

 

 

 

 

No, it will not stain the mold.

Share this post


Link to post
Share on other sites

I've had mason stain -- mixed with a porcelain slip made from clay and applied as decoration on slabs -- leave color stains on plaster hump/slump molds. I know there are body stains -- that are added to white slip for coloring -- but have not used them in molds.

Share this post


Link to post
Share on other sites

I think it would be best to try it on an old slip mold first. Whenever I use my red slip it stains the molds and almost everything else. So much that I use specific molds just for my redware slip.

 

I see you're in Colorado. If you don't have an old or extra slip mold if you want send me a message with your email or address and I'll mail one out to you. I'm in Centennial.

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.