I'm certain I'm not the first to ask this, but can't find any posts on it... Feel free to link me to the right thread....

I just got a dark clay and am also using a white clay. How do you organize your clays/throwing days to keep them and their dust/sediment/recycling separate?

Thanks.

Link to post
Share on other sites

I tried for a bit, but I noticed that my white stoneware and porcelains look good when thrown with the same slip and water I use for my red stoneware.  It's only enough to give it a slight funk, but i think it looks real nice.  

For wedging I use a 2x2 sheet of Baltic birch plywood and I would keep one side for red and one side for white, and just flip it on my wedging table.  Now I don't even bother with that.

Here's an example of porcelain thrown with a little red stoneware throwing water.  There was enough iron in the surface to overcome the very light copper coloration in the glaze.

8lDbpc5.jpg

Edited by liambesaw
Link to post
Share on other sites

Interesting on th' colour mix Liamb!

How thorough the clean has been dependent on how much colour change, most thorough on change to white and after black; hence, the white and black - also red - runs are longest. I've separate wedging boards for white, red, buff-ish, black. 

Link to post
Share on other sites

Very hard always s pollution...esp from under wheel head when you think you have it all.

Suggest a long run of one then with separate boards buckets sponges bats and scrupulous wheel head and splash pan clean...even then.

Or do a middle run of pots where you dont cate.......until you get the "pure".

Mark's way the only way for sure.

Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.