Marlene Ingenthron Posted March 10, 2020 Report Share Posted March 10, 2020 I glazed a ceramic piece inside, painted and glazed the outside. When we fired it for horse hair, all went well. Several minutes after the horse hair was finished all the paint started to fall off. What did I do wrong?? Link to comment Share on other sites More sharing options...
Min Posted March 13, 2020 Report Share Posted March 13, 2020 Could you give a bit more information on the glaze you used and post some pictures? Typically glaze isn't used for horse hair raku. Welcome to the forum Link to comment Share on other sites More sharing options...
Dick White Posted March 13, 2020 Report Share Posted March 13, 2020 Further to Min's comment, you say you glazed the inside and painted and glazed the outside. What did you paint it with? I am confused by your use of both words "paint" and "glaze." Link to comment Share on other sites More sharing options...