I have tissue and wish to print an image or text onto it. Then transfer this onto the clay.

 

The ones I currently use are pre printed, These are placed onto the clay the back is brushed with water then tissue is peeled away>

 

Thanks

 

 

 

Mike

Share this post


Link to post
Share on other sites

and your question is?

 

 

 

 

Have tissue and wish to print an image or text onto it. Then transfer this onto the clay ?

 

Ok, how do I preint the image onto the tissue, Prefer Printer if possible. Any ideas on the type of Ink???

 

 

 

Regards

Share this post


Link to post
Share on other sites

I agree with INYA.

What is your question?

Marcia

 

 

 

Have tissue and wish to print an image or text onto it. Then transfer this onto the clay ?

 

Ok, how do I preint the image onto the tissue, Prefer Printer if possible. Any ideas on the type of Ink???

 

 

 

Regards

Share this post


Link to post
Share on other sites

This has been covered-use the search or google it-I recall printer details etc.

Mark

 

 

 

ive searched and found nothing

Google only comes up with pre printed or the sliding type transfer.

 

 

 

Thanks

Share this post


Link to post
Share on other sites

This has been covered-use the search or google it-I recall printer details etc.

Mark

 

 

 

ive searched and found nothing

Google only comes up with pre printed or the sliding type transfer.

 

 

 

Thanks

 

think they meant search here on forum too

Share this post


Link to post
Share on other sites

Mitch Lyons applies colored slip to newsprint, then transfer it to clay slabs. He has a video demonstrating the process.

 

Here is another approach:

 

 

 

Thsi is NOT Slip.

 

 

Its Images and or patterns on Tissue paper.

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.