Recommended Posts

They shouldn't explode Lee. Terracotta is porous so it's easy for any moisture to escape. I'ld put a test piece or even some shards of the same type of pot in a saucer and fire it up to ^04 and see what happens. If the pots are Mexican terracotta they could be made from a really lowfire clay.