Tough to answer that question actually. Experience is best, trials are the best way and test tiles with good notes are super important. Experienced potters can tell you a lot of general properties of their glaze, but then again they have acquired the experience. Generalities for a celadon for instance might be darker color with more dramatic breaks and at some point perhaps too thick and it runs or crawls.

Test tiles likely are the best solution, one, two, three dip and so on.

Here is a shot of about 1/5th of the tiles from a Jon Britt workshop. Took him a long time to get this experience. If you go to a workshop you likely can gather some of that experience in on tenth the time or simply exchanging info with other potters often saves a bunch of time.

you can also search https://glazy.org/search?base_type=460&production=false&photo=false Many have pictures and notes on application. All for no charge.

 

39BFD0F6-FC96-46A2-BC53-A22866DB8EE7.jpeg

Edited by Bill Kielb
Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

 Share

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.