Hi, For a bit of context I make pottery that I apply layers of slip to create a raised bumpy surface. When my work is in greenware stage the dots are easily knocked off, and although I can load my work with out knocking any off in my current studio situation Im not the one loading the kilns and I've been constantly getting pieces that have multiple dots missing. I was wondering if anyone knew of something that will help to keep attached pieces or slip trailing from being knocked off by people during loading. I was thinking maybe an organic hairspray or to coat the piece in wax

Link to comment
Share on other sites

5 minutes ago, Sean Tessandori said:

Hi, For a bit of context I make pottery that I apply layers of slip to create a raised bumpy surface. When my work is in greenware stage the dots are easily knocked off, and although I can load my work with out knocking any off in my current studio situation Im not the one loading the kilns and I've been constantly getting pieces that have multiple dots missing. I was wondering if anyone knew of something that will help to keep attached pieces or slip trailing from being knocked off by people during loading. I was thinking maybe an organic hairspray or to coat the piece in wax

The only thing I've found that works really well, is to use your clay body as the slip, and apply the slip immediately after throwing while it's still green.  Don't wait til leather hard or use a mixed slip. It would be difficult to match wet->dry shrinkage between your clay body and a slip that is mixed.

Link to comment
Share on other sites

I'ld try mixing up the slip with part water and part magic water. The sodium silicate in the magic water helps the clay surface dry hard. Would have to try a few tests to see what ratio of water:magic water works best. Magic water recipe if you don't have it already is 1 gallon of water, 3 tablespoons of sodium silicate and 1 1/2 teaspoons of soda ash.
Welcome to the forum. 

Link to comment
Share on other sites

16 minutes ago, Min said:

I'ld try mixing up the slip with part water and part magic water. The sodium silicate in the magic water helps the clay surface dry hard. Would have to try a few tests to see what ratio of water:magic water works best. Magic water recipe if you don't have it already is 1 gallon of water, 3 tablespoons of sodium silicate and 1 1/2 teaspoons of soda ash.
Welcome to the forum. 

It's also a deflocculant so the slip can use less water and decrease shrinking

Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

 Share

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.