Recommended Posts

Help new potter here trying to make glaze ? recipe calls for / ingredients Silica 30.% Minspar38% Whiting 14% Zinc Oxide12% 0m-4Ball clay6% what am I looking for when thay ask for  Silica is there a nother word for Silica what do I use? can you help

Share this post


Link to post
Share on other sites

sherry, if you are very new to making glazes, you might not know that silica, call it whatever you like, is dangerous to your lungs.  please read all you can on the safest way to use it.

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.


×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.