I used a series of 4 glazes layered on a recent set of plates. Every single one of them has crawled, especially on one particular colour which I’m guessing is the thicker application when layered? 
My question is, can I reglaze and refire them, perhaps to a lower temperature? They’ve been fired to cone 7 (electric), and it’s a Valentine’s Delta stoneware. 

I’ve refired plates before and they’ve broken right down the centre. I’ve seen people on here say they’ve had success with refiring and wondering if there’s a recommended technique.

Attached a couple of photos of the crawling. Hoping someone with more experience than I can provide a helpful suggestion. Other than telling me not to layer the glazes! Funnily enough I’ve used this glazing technique plenty of times on bowls without any problem.

 

Thanks in advance. 

AAA4625A-B07C-40BA-B73D-51CECBB35488.jpeg

C5A729B9-B013-4B0F-ADD3-5891758C3E12.jpeg

Edited by roobarb
Spelling
Link to comment
Share on other sites

In the area where the glaze pulled away, you might take a grinder (Dremel with a diamond bit), then reglaze just that area. It looks like the rim is unglazed.. If that's the case, you might fire them rim down. I've had success with grind, reglaze and refire, but it was with very small bare spots. 

Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

 Share

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.